Die casting is a manufacturing process that uses high-pressure molten metal to create intricate metal parts. It is a versatile process that can be used to produce a wide variety of parts, including automotive components, electronics housings and medical devices.
While die casting is a reliable process, it can sometimes produce defects. This article discusses some of the most common die casting defects, their causes and solutions.
Die casting defects
When zinc die casting first became available, it quickly gained recognition as a lightweight and cost-effective alternative to other alloys such as tin and lead. Over the past century, zinc alloys have made steady progress. While zinc has always been acknowledged for its high strength, the introduction of the Zamak family, and now the revolutionary EZAC™ alloy, has further enhanced the suitability of zinc alloys for hot chamber die casting across a wide range of applications. Prior to the introduction of EZAC™, zinc was often overlooked for applications requiring high tensile strength, especially high-temperature tensile strength. Additionally, most zinc alloys exhibited low creep resistance compared to other materials. These areas of improvement were the primary focus during the creation of EZAC™, resulting in a zinc alloy that surpasses previous limitations.
Heat check
A heat check is localised cracking or surface damage that can occur on the die casting mould. It is caused by thermal stress and cycling, which can be exacerbated by factors such as inadequate cooling, excessive overspray or thick mould sections.
Soldering
Soldering is the formation of a thin metal layer on the casting surface. It is caused by erosion or dissolution of the die material due to uneven cooling, localised high temperatures or improper metal flow. Soldering can be prevented by improving cooling, optimising part design, and improving metal flow management.
Cracks
Cracks are fractures or separations that can occur in the die casting. They can be caused by stress concentration, rapid cooling and uneven thermal gradients. Cracks can be minimised by evaluating casting geometry, adjusting process timing and enhancing thermal management.
Dimensional concerns
Dimensional concerns involve deviations from the desired dimensions and tolerances in the die-cast part. They can be caused by unrealistic drawing tolerances, variations in process parameters and thermal expansion effects. Dimensional concerns can be minimised by optimising tolerances, controlling process parameters and considering thermal effects.
Flash
Flash is excessive material that escapes between mould halves, forming thin fins or flanges on the casting. It can be caused by insufficient machine tonnage, die wear or misalignment, and suboptimal process parameters. Flash can be prevented by ensuring adequate machine tonnage, conducting regular die maintenance and optimising process parameters.
Shrink porosity
Shrink porosity is characterised by voids or cavities formed due to the shrinkage of molten metal during solidification. It can be caused by non-uniform wall thickness and abrupt section transitions in the part design. Shrink porosity can be minimised by optimising casting geometry and implementing effective thermal management.
Flow marks (cold flow, non-fill, etc.)
Flow marks appear as visible lines or streaks on the casting surface due to the flow of molten metal during mould filling. They can be caused by flaws in part geometry and inadequate gate and runner design. Flow marks can be minimised by refining part geometry, using flow simulation software and implementing real-time monitoring.
A comprehensive understanding of common die casting defects, their causes and practical solutions is pivotal in engineering high-quality castings. By implementing the solutions discussed in this article, manufacturers can effectively address defects, enhance production efficiency and deliver products that meet exacting quality standards.